搜索结果: 1-14 共查到“医学 Debonding”相关记录14条 . 查询时间(0.048 秒)
Modification of 4-META/MMA-TBB Resin for Safe Debonding of Orthodontic Brackets — Influence of the Addition of Degradable Additives or Fluoride Compound
4-META/ MMA-TBB resin Debonding Enamel
2009/9/14
The purpose of this study was to evaluate the performance of modified 4-META/ MMA-TBB resin cements (Superbond C&B) in terms of debonding orthodontic brackets easily and safely from enamel without the...
Development of an Easy-debonding Orthodontic Adhesive using Thermal Heating
Debonding Orthodontic adhesive Microcapsules
2009/9/14
We produced experimentally a new bonding material that consisted of a mixture of a base resin (4-META/MMA-TBB resin adhesive) and thermoexpandable microcapsules for safe, easy debonding. Microcapsules...
Enamel bonding of self-etching and phosphoric acid-etching orthodontic adhesives in simulated clinical conditions: Debonding force and enamel surface
Self-etching Phosphoric acid-etching Orthodontic adhesive
2009/9/11
This study aimed to evaluate the effectiveness of self-etching and phosphoric acid-etching orthodontic adhesives for enamel bonding in simulated clinical conditions. By using two self-etching (Transbo...
Lip Posture Following Debonding of Labial Appliances Based on Conventional Profile Photographs
Photographs Profile Lip posture Analysis
2010/3/5
Objective: To assess changes in lip posture following debonding of labial appliances on the basis of a new soft tissue analysis performed by computerized tools with the use of conventional nonstandard...
Finishing of Enamel Surfaces after Debonding of Orthodontic Attachments
Enamel Surfaces Debonding of Orthodontic Attachments
2009/3/8
Finishing of Enamel Surfaces after Debonding of Orthodontic Attachments.
Debonding forces applied to ceramic brackets simulating clinical conditions
Debonding forces Ceramic brackets Pliers Shear test
2009/1/12
Debonding ceramic brackets is an area of concern to clinicians. Reports of enamel fractures and cracks have raised questions about the safety of the procedures used to remove these attachments.
Experimental traumatic debonding of orthodontic brackets
Traumatic Debonding Ceramic brackets
2009/1/12
This study was designed to gather information on enamel damage concomitant with traumatic debonding of orthodontic brackets. Seventy-eight extracted premolars passed an inspection for defects and ...
Enamel surfaces after orthodontic bracket debonding
Enamel surfaces Scarred enamel Post-debonding polishing
2009/1/12
The enamel surfaces of extracted teeth were studied clinically and with a scanning electron microscope following debonding of orthodontic attachments and subsequent polishing. Excess orthodontic r...
Stresses developed during clinical debonding of stainless steel orthodontic brackets
Orthodontic brackets Debonding Dental stress analysis
2009/1/8
The purpose of this project was to use finite element modeling to calculate and compare the peak stresses generated during clinical debonding of resin bonded brackets. Five debonding techniques we...
Comparison of bracket debonding force between two conventional resin adhesives and a resin-reinforced glass ionomer cement:An in vitro and in vivo study
Bond strength Composite resins Glass ionomer cement
2009/1/7
The purpose of this study was to compare the debonding force of orthodontic brackets bonded with two conventional resin adhesives (Resilience L3 and Light Bond) and a resin-reinforced glass ionome...
Effect of resin cure mode and fluoride content on bracket debonding
Orthodontic resin Polymerization mode Shear debond Fluoride
2009/1/7
Enamel decalcification around brackets is sometimes observed during and after orthodontic treatment. Reports in the literature suggest that the preventive advantage of fluoride-releasing adhesive ...
Bracket bonding with 15- or 60-second etching and adhesive remaining on enamel after debonding
Brackets Bond strength Enamel etching Debonding
2009/1/4
The purposes of this study were to (1) evaluate the shear bond strength of brackets fixed to enamel that has been etched for 15 or 60 seconds, (2) correlate etch time with amount of resin remaining ...
Possibility of Blood and Hepatitis B Contamination Through Aerosols Generated During Debonding Procedures
Aerosols Occult blood Infectious agents Viral infections Hepatitis B.
2008/12/19
The primary purpose of this study was to investigate the presence of blood or blood elements in aerosols generated during the debonding procedures. The presence of three hepatitis B carriers in th...
Shear Bond Strength and Residual Adhesive after Orthodontic Bracket Debonding
Orthodontic brackets Resin-modified glass ionomer cement Shear bond strength Residual adhesive
2008/11/20
Objective: To compare the shear bond strength and determine the area of residual adhesive on teeth after the debonding of brackets bonded with two types of orthodontic adhesives. These were a resin-...